Nanophotonics

Cathodoluminescence (CL) imaging is a powerful method for studying optical phenomena at the nanoscale. The electron beam acts as a very pure local excitation source. The hyperspectral light-emission maps produced with CL illustrate the local density of electromagnetic states, a quantity that determines how well light couples to matter and vice versa. Furthermore, the directionality and polarization of emission can rigorously be measured with angle-resolved images, thus providing yet more insight in the optical properties of nanostructures.

This makes the technique highly relevant to the field of nanophotonics. It is applicable to metallic as well as dielectric and semiconductor nanostructures, including nanoparticles, nanowires, metamolecules, metasurfaces, and photonic crystals. These structures find applications in (bio)sensing, fluorescence enhancement, non-linear optics, low-threshold steam generation, LED’s, solar cells, integrated photonics, lasers and much more.


 Imaging of the Modal Dispersion of Light

Nylon Thread 

By periodically altering the refractive index of a material on the scale of the wavelength of light, a photonic crystal can be made which exhibits interesting optical properties.

How light propagates through such a material can manifest itself in an angular diffraction pattern which can be measured using angle-resolved cathodoluminescence.


Spatial Characterization of angular emission from nanoantennas

Nylon Thread 

Metallic nanowires or nanoridges support a guided surface plasmon mode. At the end-facets these waves can be reflected leading to a standing-wave resonance.

Such nanoscale resonant modes can be imaged with hyperspectral cathodoluminescence imaging.


Related Pages

Cathodoluminescence
Cathodoluminescence

Modular CL in-SEM system with multiple imaging modes


Applications

Contact An Applications Scientist


 

Captcha Code

Click the image to see another captcha.